Water seeps through mortar cracks because several forces can move water through an opening at once. A joint crack lets rain reach the inside of the masonry, and once water is in the gap it can be pulled further in by capillary suction, pushed by air pressure from wind or drawn down by gravity. The mortar joint is usually the weakest part of a brick or block wall, so it is where cracks most often appear. This guide explains the mechanisms that published research describes and what the sources do not settle.

At a glance

  • Wind-driven rain pushes water against a wall at an angle. Cracks, voids and pores in the surface give that water a way in.
  • Very narrow openings draw water in by capillary suction. A Lund University thesis says this matters most for openings smaller than 0.5 mm.
  • Mortar is designed to be the sacrificial part of a wall. It is cheaper and easier to repair than the bricks it holds.
  • The sources give repair criteria, but they disagree on the crack width that matters, so a single number is not a safe rule.

What the wall is made of

Mortar is a workable paste that hardens to bind building blocks such as stones, bricks and concrete masonry units. It also fills the irregular gaps between units and spreads their weight evenly. According to the Wikipedia overview of masonry mortar, the mortar “functions as a weaker component than the building blocks and serves as the sacrificial element in the masonry, because mortar is easier and less expensive to repair than the building blocks.” That design choice explains much of the pattern. The joint shrinks, ages and cracks, while the brick stays in place.

Mortar type also matters. The same overview notes that lime mortar is softer than cement mortar, which lets brickwork move a little with shifting ground. Where a hard cement mortar sits next to softer lime, the brickwork can crack. Lime mortar is described as breathable, meaning moisture can move through it and evaporate from the surface, while cement mortar can stop that evaporation. These are general properties described in background sources, not measurements of any particular wall.

How rain gets through a crack

Rain does not usually fall straight onto a wall. When wind blows, rain strikes the surface at an angle, which is called oblique driving rain. The Lund University thesis by Kahangi (2021) on clay brick facades describes this directly. It says the combination of wind and rain “together with the presence of deficiencies like cracks, voids, and pores, may result in water penetration.”

The same thesis lists the factors that control how much water reaches the wall. The first group is about the rain itself: rain intensity, raindrop size, wind speed and direction, building geometry and height, and topography. The second group is about the wall: the presence of cracks, the profile of the mortar joints, the type and quality of the masonry units, the type of mortar, joint thickness and workmanship. A crack on a sheltered side of a building may leak very little, while the same crack on the windward face can take much more water.

Once a crack exists, the thesis gives three possible driving forces. These are capillary suction, air pressure differences caused by wind, and hydrostatic pressure from gravity. It notes that for openings smaller than 0.5 mm, capillary suction seems to be important. The thesis calculates that capillary suction for cracks between 0.1 mm and 1 mm wide would be in the range of 75 to 750 Pa. That range is a calculation from the thesis, not a field measurement from this site.

Crack width: what the research cites

Crack width is the number most people look for, and the thesis shows why a single figure is hard to apply. It reports that Birkeland claims water penetration occurs when cracks with 0.1 mm to 5 mm width exist. Grimm categorizes interfacial cracks generally ranging between 0.1 and 1 mm. Those two ranges overlap but are not the same.

The thesis also reviews repair criteria proposed by several researchers. One set recommends repointing when hairline cracks appear on the mortar surface, when joints are eroded to a certain depth, when crack widths larger than 2 mm have been measured, or when water absorption is more than 4.5 l/m2/h. The thesis then questions the 2 mm figure. It states that “water ingress in cementitious materials increases exponentially when the crack width exceeds 0.2 mm.” In other words, the cited criteria do not agree with each other about where the risk starts.

The thesis also points out that repointing removes only the outer part of a joint. It says that only 25 mm of the outer part of the cracked or eroded mortar joints, or 2.5 times the mortar joint thickness, is normally raked out and replaced. Whether a surface repair reaches the depth that feeds the leak is a question the thesis says needs investigation.

What remains unclear

The sources do not give a single safe crack width for every wall, and we did not add one. They also do not give a field test that a homeowner can run to tell whether a particular crack is leaking. The thesis describes washing a wall to reveal the depth of erosion and cracks, and it mentions surface grouting for hairline cracks that are not deep. Neither source gives a step-by-step method for doing this, so this page does not offer one.

What the sources do not say

The sources do not give a price, a product, or a repair timeline. They do not say how long a hairline crack takes to become a leak, and they do not compare cost of repointing against surface sealing for a specific wall. The thesis was written for clay brick facades, and the Wikipedia overview is general, so neither should be read as a guide to a particular building code or climate.

Frequently asked questions

Does every mortar crack let water in?

No. The thesis describes water penetration as depending on rain exposure, wind direction, the wall’s construction and the crack’s size and depth. A hairline crack on a sheltered wall may leak very little, while a wider crack on a windward face may take in much more water.

Why does water sometimes come out on the inside of a wall?

The sources in this page do not explain interior wetting in detail. The thesis lists water infiltration on interior walls as one sign that repointing may be needed, but it does not trace the path through the wall for any specific case.

Is lime mortar better than cement mortar for cracks?

The Wikipedia overview says lime mortar is softer, more flexible and breathable, while cement mortar is harder and allows little flexibility. The sources do not rank them for leak resistance, so this page does not give a ranking.

What crack width should I repair?

The sources disagree. The thesis cites a 2 mm repair threshold from some researchers and questions it, citing research that water ingress increases exponentially above 0.2 mm in cementitious materials. The sources do not give one universal number.

Does repointing stop all leaks?

The thesis says that repointing removes only the outer part of a joint and that the link between erosion depth and water intake needs examination. It does not claim that repointing stops every leak.

For related water-movement topics, see how to assess soil drainage and how to make a rain garden in your backyard.