Thermal expansion cracks form in concrete when temperature changes make the material grow and shrink, and the parts inside the mix do not move together. Concrete is built from cement paste, fine aggregate and coarse aggregate, and each part responds to temperature differently. That mismatch creates tensile stress, which can start microcracks at the weak points in the mix. This explainer walks through that mechanism using two research papers on concrete thermal behavior and notes where those papers stop.

At a glance

  • Concrete expands when it warms and contracts when it cools, and its internal parts do not change by the same amount.
  • Temperature changes in either direction can create tensile stresses inside the material.
  • The thin zones of cement paste around aggregate particles are the weakest links, so microcracks are described as starting there.
  • Large pours can also crack while they are young because of heat released as cement hydrates. That is a related but separate cause.

What concrete is made of, and why that matters

Researchers who model concrete treat it as a set of separate constituents rather than one solid block. One modeling study introduces the cement paste, the fine aggregates, the coarse aggregates and the interfacial transition zones as elementary constituents of concrete. The interfacial transition zones are the places where paste and aggregate meet. The same study describes them as thin layers of the porous cement paste covering the aggregates.

This split matters for temperature because each constituent can respond differently. The study notes that the thermal expansion coefficient of mature concrete depends on the aggregate type, the volume fractions of the constituents, the age and the internal relative humidity. In other words, two concretes do not necessarily expand by the same amount. A mix with a different share of aggregate, or a different aggregate, can behave differently when the temperature changes.

Aggregate choice is a large part of this. The same study says that the type and the volume fraction of coarse aggregates were shown to be particularly important for the values of the thermal expansion coefficients of concrete. It also states that aggregates with a rich content of quartz have larger thermal expansion. For a reader, the practical point is that the mix itself is part of the mechanism, not just background detail.

How temperature change produces stress

When the temperature changes, the parts of concrete try to change size. The modeling study explains that microscopically inhomogeneous thermal deformations occur at temperature variations as a result of the heterogeneity of concrete. In plain terms, the deformation is not the same across the material, and that unevenness is where the stress comes from.

Both directions matter. The same study states that both a decrease and an increase of the temperature can result in microscopic tensile stresses, either in the bulk cement paste or in the interfacial transition zones. So a slab can be stressed on a cold night and again on a warm afternoon. Heating is not the only trigger that the study identifies.

The study then links that stress to damage. It states that this leads to microscopic thermal stresses and to microcracking. Microcracks are small cracks inside the material, and they are the first step the study describes. The same paper describes cracking of the cement paste, induced by tensile stresses, as a serious threat for the long-term durability of concrete structures.

Where the cracks are described as starting

The weakest part of the mix is the boundary between paste and aggregate. The modeling study describes the interfacial transition zones as the weakest links in the microstructure of concrete. That description is why the boundary zones are the first place to look when the question is where a crack begins.

The study works at the scale of the microstructure, so its findings describe what happens inside the material. They do not give a crack timeline for a particular slab, and they do not say how quickly microcracks grow into visible cracks in a patio. Those gaps are covered in the section on what the sources do not say.

Early-age cracks in thick concrete

A second, separate mechanism applies to large pours. A procedure paper on early-age thermal cracking explains that cracks in early-age mass concrete structures caused by hydration heat are a well-known phenomenon that affects their serviceability, durability, and tightness. It states that the primary cause of these cracks is the uneven temperature rise within the structure due to the exothermic nature of cement hydration.

The same paper describes the cause in slightly different words: the primary cause of these cracks is inhomogeneous volume changes due to thermal and moisture gradients during the cement hydration process. The uneven temperature rise is the central idea. Heat from the cement reaction raises the temperature inside the element, and the volume changes that follow are not uniform.

The paper defines mass concrete as any volume of concrete with dimensions so large that measures must be taken to reduce the risk of cracking due to volume changes from the heat generated during hydration. It also states that the risk of cracking is generally assessed by comparing the tensile strength of concrete with the thermal stresses induced in mass concrete structures. For prevention, the most common approach it names is to optimize the concrete mix design by using low-heat cement or incorporating supplementary cementitious materials.

This early-age mechanism concerns mass concrete, which is defined by size. The definition is the reason it is kept separate from the everyday temperature-swing mechanism described earlier in this explainer. Both mechanisms involve tensile stress, but the paper ties its cause to cement hydration heat rather than to the weather.

For a related but different cause of concrete cracking, see how freeze and thaw cycling cracks a concrete patio. For the chemical changes that happen inside concrete over many years, see how concrete carbonation reduces its alkalinity.

What remains unclear

The sources do not confirm crack timelines for backyard patios, expansion values for a specific home mix, or how often a given slab cracks in real weather. The two sources are engineering studies, and their numbers do not carry over directly to a garden setting.

What the sources do not say

The modeling study focuses on mature concrete and does not give a patio-scale example. The procedure paper focuses on early-age mass concrete and does not address thin slabs. Neither source gives a rule for joint spacing, a safe temperature range for pouring, or a maintenance schedule. Those points are outside what this explainer can support.

Frequently asked questions

Does concrete expand when it gets hot?

The modeling study refers to a thermal expansion coefficient for mature concrete. It states that this coefficient depends on the aggregate type, the volume fractions of the constituents, the age and the internal relative humidity.

Can concrete crack when it gets cold?

Yes, according to the modeling study. It states that both a decrease and an increase of the temperature can result in microscopic tensile stresses, and that these stresses lead to microcracking.

Why do large concrete pours crack when they are young?

The procedure paper says the primary cause is the uneven temperature rise within the structure due to the exothermic nature of cement hydration. Heat from the cement reaction is the trigger it names.

Does the type of aggregate affect cracking?

It affects the expansion behavior that drives the stress. The modeling study says the type and volume fraction of coarse aggregates were shown to be particularly important for the thermal expansion coefficient, and that aggregates with a rich content of quartz have larger thermal expansion.

Does thermal expansion explain every crack in a patio?

The sources do not say that. They describe thermal stress and early-age hydration heat in concrete, and they do not survey the causes of every patio crack.

Sources

  • Multiscale Thermoelastic Analysis of the Thermal Expansion Coefficient and of Microscopic Thermal Stresses of Mature Concrete. https://pmc.ncbi.nlm.nih.gov/articles/PMC6747584/
  • Multi-Step Procedure for Predicting Early-Age Thermal Cracking Risk in Mass Concrete Structures. https://pmc.ncbi.nlm.nih.gov/articles/PMC11313579/

Similar Posts